All I did was put tacky tape in the holes to guard from bag rips…and the tacky tape melted and flowed in all corners :-/ Been pulling on it for an HOUR now.
sunvua.
http://imgur.com/mhOHE (because the upload thingy ain’t working)
All I did was put tacky tape in the holes to guard from bag rips…and the tacky tape melted and flowed in all corners :-/ Been pulling on it for an HOUR now.
sunvua.
http://imgur.com/mhOHE (because the upload thingy ain’t working)
thats a mess! good luck
Sure looks like a bit of a mess… what process & materials were you using?
At least you have now tested that type of tape…!
Not sure of the tape, but it’s from GS, and we use it to 400f. This was at 150f for 16hr…I don’t normally have a complex shape like this, but damn did it flow to everywhere there was a void.