Just want to say this product works extremely well. Easy to cure and is easily washed out. Much better than high temp salt pour. It can be easily formed for core when packed into a starter mold. It bakes at 200f and if brought to temp slowly doesn’t crack out. Also can be hand formed.

I highly recommend this product.

Also infuses just fine. And accepts prepreg and wet layup just fine. Slows cures down a bit as it hold heat but that’s the only draw back.

Works excellent for building proto parts and quick tooling fabrication.

Google aquacore 6001 to get it if you need an easy wash out solution.

Im trying to find where i can get it in the uk i would like to try this making pipe with bends

Does it have to be baked ?

Or evan a cycle frame :wink:

Yes it needs to be baked

It would work great for pipe with bends. But tooling costs would be high. As this would be a consumable. Why can’t you get it shipped to the UK?

I probably can but pointless if it needs to be baked :confused: