anyone ever infuse with Zylon instead of carbon?

I’m curious, I like the look of the gold color it has and it would look great on some parts for a friends bike, but I have never heard of anyone using it as reinforcement. I have read that it is UV sensitive, as far as it’s strength goes… but this would be unimportant in cosmetic parts.

Any advice or suggestions as far as infusing it ? any personal experiences?

You can get gold coloured Eglass, which is exactly the same as the silver, but different colour. I have some which is gold on one side, and silver the other…

http://www.sri.com/psd/poulter/air_safety/as_gifs/air_frag.GIF

haahaahaa!!!

Anyways, is it gold, or just dark yellow?
shrugs if only for a surface layer, I’m sure it’ll work.

I have yet to find a seller in North America…