Any experience with ORCA 511 VE INFUSION RESIN

ORCA 511 VE INFUSION RESIN
http://www.fiberlay.com/prod-polyesters.php?subclass=050%20051%20052%20053%20054%20055&startrow=30

Looks like the physicals of this resin are quite suitable for decent body panels.

Good low viscosity at ~sub 150 cps

good HDT of 239F

Anyone have experience with this VE for infusion?

What would be an expected post cure for something like this? Any ballpark ideas of shrinkages that such a VE may have once pulled from a mold?

Thanks.

Bump? Interested in results.

Ya for 2 years lol.

I haven’t used it but definitely interested… Still…