Anti-symmetric composites application

Hi
Actually, I am studying the impact of nanofillers on Anti-symmetric composites. Therefore, composite samples with layup sequence as [+45/ 0 / 0 / 90 /90 / 0 /0/-45] were fabricated and tested.I am wondering the excellent strength enhancement. Specifically, by using of SWCNTs and GNPs the UTS is enhanced by 40% 30% ,respectively. In addition, 9 % improvement in ILSS.

So, what is the suggested applications for this composite type .

I really appreciate any help you can provide